Nickel alloys TIG ERNi-I solidatorium nexum
CHEMICAL COMPONET:
ADMISSUS (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Ti | P | S |
GB/T REGULAE | 0.15 | 1.00 | 0.70 | - | ≥92 | - | 1.0 | 2.0-3.5 | 0.03 | 0.014 |
AWS Rules | 0.15 | 1.00 | 0.75 | - | ≥93 | - | 1.0 | 2.0-3.5 | 0.03 | 0.014 |
EXEMPLUM PENSI HABEO | 0.005 | 0.48 | 0.26 | 0.46 | 94.69 | 0.001 | 0.07 | 2.95 | 0.001 | 0.001 |
MACHINA proprietas:
POSSESSIO | VICTORITAS (MPa) | PROLATIO VIS (MPa) | IMAPACT VALEO J/℃ | PROLATIO(%) | ||||
GB/T REGULAE | - | - | - | - | ||||
AWS Rules | - | - | - | - | ||||
EXEMPLUM PENSI HABEO | - | 550 | 276/-196 | 36 |
Purus nickel gas glutinum filum, compositio nominalis 96%Ni-3%Ti.
Ob additionem sufficientis elementi, porositas efficaciter minui potest in processu glutino.
Arcus stabilis, pulchra formans, bonum fluxus ferri fusilis, processu egregio glutino effectus.
-
37,000 tons generale navis onerariae
-
JU2000E jack-sursum EXERCITATIO rig
-
Salus iniectio arca
CHEMICAL COMPONET:
ADMISSUS (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Ti | P | S |
GB/T REGULAE | 0.15 | 1.00 | 0.70 | - | ≥92 | - | 1.0 | 2.0-3.5 | 0.03 | 0.014 |
AWS Rules | 0.15 | 1.00 | 0.75 | - | ≥93 | - | 1.0 | 2.0-3.5 | 0.03 | 0.014 |
EXEMPLUM PENSI HABEO | 0.005 | 0.48 | 0.26 | 0.46 | 94.69 | 0.001 | 0.07 | 2.95 | 0.001 | 0.001 |
MACHINA proprietas:
POSSESSIO | VICTORITAS (MPa) | PROLATIO VIS (MPa) | IMAPACT VALEO J/℃ | PROLATIO(%) | ||||
GB/T REGULAE | - | - | - | - | ||||
AWS Rules | - | - | - | - | ||||
EXEMPLUM PENSI HABEO | - | 550 | 276/-196 | 36 |