620Mpa manu Electrode quia Fortitudo Steel
Applicationem & Standard
1. Apta ad stannum chalybis demissa aurum, medium carbo carbonis glutino, ut machinas fabricas, machinas portus et alias occasiones.
2. Vexillum occurrit: GB/T32533 E5918-G P, AWS A5.5 E9018-G & A5.5M E6218-G, ISO18275-A:E 55 5 1.5NiMo B 3 2, ISO18275-B: E6218-G P
Preheating et inter-canale temperies: 150±15℃, curatio caloris ad coagmentationem materialium normarum requisitorum, 620±15℃*1 hora post-conventio curationis caloris.
E9016 genus potassium hydrogenii humile est pharmacum genus cutis humilium mixturae altae roboris ferri electrode, AC et DC dualis usus, AC welding in stabilitate praestanda, paulo inferior DC glutino, ad glutino mediae carbonis adhibito et viribus inferioris respondentis. admiscent alta vi ferro compaginem, ut 15MnVN ferro. Electrode ante glutino ad 350℃ pro 1h coquendum est, et postea cum coquendo utendum est. Si crassa pulvis est, supra 150 urendus est et post glutino tardius refrigerandus.
Features
1. Pulvis ferreus humilis hydrogenii manus electrode, efficientia alta, arcus stabilis, parva adipiscing, bona formans, facile deducens, X-radius effectus est excellens.
2. Vox resistentiae ac stabilis proprietates mechanicas habet.
J606 altae vires chalybeis electrode exemplar: E9016-G altum robur ferri electrode notae: humilis hydrogenii potassium genus humilis mixturae altae vires ferri electrode, AC et DC usus dualis, glutino potest esse in plena positione, AC glutino processu perficiendi stabilitate aliquantulum inferior. dc glutino. Propositum: Medium carbonis chalybeum et admixtum vi gradus altae fortitudinis ferro respondentem, ut 15MnVN.
Company & Factory
Product compositionem et proprietates mechanicas introductio
CHEMICAL COMPONET:
ADMISSUS (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
GB/T REGULAE | - | ≥1.00 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | - | - | ≥0.10 |
AWS Rules | - | ≥1.01 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | 0.03 | 0.03 | ≥0.11 |
EXEMPLUM PENSI HABEO | 0.093 | 1.258 | 0.28 | 0.03 | 1.65 | 0.42 | 0.011 | 0.007 | 0.01 |
MACHINA proprietas:
POSSESSIO | VICTORITAS (MPa) | PROLATIO VIS (MPa) | HEATTREAMENT℃xh | ||||||
GB/T REGULAE | 490 | 590 | 620*1 | ||||||
AWS Rules | 530 | 620 | 620*1 | ||||||
EXEMPLUM PENSI HABEO | 600 | 685 | 620*1 |
PARAMETERS WELDING RECOMMENDED:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
ELECTRICITY | H/W | 80-110 | 110-130 | 130-180 | 180-230 | ||||
(Amp) | O/W* | 50-80 | 90-120 | 130-160 | - |
NOTE:
H / W: situ glutino
O / W: super-caput situ glutino
Causae typicae
Testimonium
Product compositionem et proprietates mechanicas introductio
CHEMICAL COMPONET:
ADMISSUS (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
GB/T REGULAE | - | ≥1.00 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | - | - | ≥0.10 |
AWS Rules | - | ≥1.01 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | 0.03 | 0.03 | ≥0.11 |
EXEMPLUM PENSI HABEO | 0.093 | 1.258 | 0.28 | 0.03 | 1.65 | 0.42 | 0.011 | 0.007 | 0.01 |
MACHINA proprietas:
POSSESSIO | VICTORITAS (MPa) | PROLATIO VIS (MPa) | HEATTREAMENT℃xh | ||||||
GB/T REGULAE | 490 | 590 | 620*1 | ||||||
AWS Rules | 530 | 620 | 620*1 | ||||||
EXEMPLUM PENSI HABEO | 600 | 685 | 620*1 |
PARAMETERS WELDING RECOMMENDED:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
ELECTRICITY | H/W | 80-110 | 110-130 | 130-180 | 180-230 | ||||
(Amp) | O/W* | 50-80 | 90-120 | 130-160 | - |
NOTE:
H / W: situ glutino
O / W: super-caput situ glutino